Provides a durable anodized surface - which can easily be dyed.
Simple to operate - Predictable consistent results
Low Current Density means – Inexpensive power source
Low Current Density means – No heat buildup in the tank
VERY dilute chemical requirement – Environmentally friendly
No fumes – SAFER in confined areas
Fully Expandable - Kits can be made bigger by obtaining larger plastic containers
Conforms to Mil Spec A 8625 F
Standard Kit Contains:
6 x 6 gal tanks with locking rings and lids (12" diam x 14" deep)
5 tanks for the Anodizing & Dying Process, 1 tank for Anodize Stripping
4 x 300 watt Ceramic Heaters
1 x Thermostat
2 x 200 Watt Glass Heaters
1 x Rinsing Sprayer
1 pack Mist Balls
1 x 4oz Mist Suppressant – treats 48 gals of Anodizing Solution
1 x 1lb Anodizing Sealant – makes 8 gallons
1 x 2lb SP Degreaser – makes 4 gallons
2 x 1 qt De-oxidizer – makes 4.5 gallons
2 x 8" x 8" GP Plates
1 x Agitator Pump [ Not supplied in Australia]
6 x Aluminum Strips (1 for tank bar, 5 for testing)
2 x 1lb Anodize & Chrome Stripper - Makes 6 Gal
1 x Color Wheel
The Caswell Plating Manual
LCD Anodizing Instructional DVD
Requires 1 gallon Battery Acid – not supplied
At this stage of the process the film has microscopic pores which have to be sealed (or 'fixed') by dipping the part into sealer for 15 minutes. The part may be colored prior to boiling by simply soaking in our range of professional anodizing dyes. An almost infinite range of colors can be produced by mixing the dyes together.
The most exciting part of aluminum anodizing, is without doubt, experimenting with the amazing array of colors and effects one can produce, with a little practice and skill. The metal can be pretreated in a variety of ways, polished, scratch brushed etc., the anodize film grown, and then the colors applied prior to sealing the anodize surface, permanently locking the colors into the metal. The system is ideal for paint ball guns, model aircraft parts, and prototype work. The manual and DVD discuss the numerous techniques for dyeing, including multicolor, ‘splash’ dyeing, silk screen printing, air brush spraying etc.
Each kit is supplied with a color wheel. Dyes can be mixed together to create a host of different colors. The dyes are in concentrated liquid form, a 4oz bottle makes up 2 gals of ready to use dye. To make up different colors, we suggest that you make up the colors to the correct dilution first, then take a quantity of each dye and blend them together. A color chart can be used here.
Anodized aluminum has a very durable surface that is unaffected by weather and many chemicals. The surface will resist high temperatures, even a blowtorch, for short periods.
The issue of safety whilst anodizing is addressed by the use of plastic fume balls and a chemical mist suppressant, both of which float on the surface of the anodizing tank. During operation, no dangerous fumes are evident. Anodize Fume Suppressant may also be used on any sulfuric acid electro-stripping or etching tanks.
Don't rely on mist suppressants entirely, they ALL break down eventually. Fume balls are permanent and they help control heat loss & evaporation, maintaining a more even tank temperature. Don't settle for kits that don't come with fume balls.