Gloss Killer
Gloss Killer

Gloss Killer

Turn any glossy powder into a semi gloss or matte powder.

For semi gloss, mix 10%-20% with your powder (1.6-3.2 oz/lb)
For matte, mix 20%-30% with your powder (3.2-4.8 oz/lb)
Do not exceed 30% mixture.
Do not use with High Temp Powders
8oz container treats 1-2 pounds of powder

 

Buy Now!
Price: $24.95
Quantity:




Contact Us:
25 Birch Court
Wyndham Vale
Victoria 3024
Phone: 03 9741 7103 or 0427 70 80 90
caswell-australia@caswellplating.com

Copyright © 2008 Caswell Australia

All Prices In Australian Dollars and Subject To Change Without Notice.

Customers Not In Australia Should Go To Caswell Inc.'s Web Site.

Customers Are Welcome To Pickup Goods From Our Location, But Please Call First To Check Product Availability
Powered by Squirrelcart © PHP Shopping Cart Software