Copy Cad® & Zinc Plating Kit
Copy Cad® & Zinc Plating Kit
All the benefits of CADMIUM & ZINC PLATING without the dangers!

No cyanides! No dangerous chemicals!

No fumes! No disposal problems

Sacrificial (cathodic) coating - Just like real Cadmium

Inexpensive - no need to deal with plating shops!

Excellent corrosion resistance!

Now, Copy Cad® AND Zinc plating in one kit. By simply adding a special brightener to the solution, the normally dull, flat, whitish look of Copy Cad® is transformed into a commercial quality bright zinc plate. After use, the bath reverts back to the original Cadmium look.

This simple system is designed to give professional results without a complicated 'chemistry set'. The kit comes with an Abrasive wheel which provides a 'flat' finish to the metal for Copy Cad® .

These kits are designed to provide a professional zinc finish to a variety of substrates on small components such as workshop tools, brake boosters, brackets and zinc alloy carburetor castings.

1.5 Gallon Kit: 2 x 2 Gal Plating Tanks & Lids 2 x 4" x 8" Zinc Anodes 1 Quart Copy Cad® /Zinc Solution (Makes 1.5 Gals) Zinc Brightener 1 Pack Degreaser, makes 4 gallons 2 x 300W Heaters 1 x Heater Thermostat Abrasive Nylon Wheel 1 x Pump Filter/Agitator [NOT INCLUDE IN AUSTRALIAN KITS] The Caswell Plating Manual Free Technical Support 3 Gallon Kit: 2 x 3.5 Gal Plating Tanks & Lids 2 x 4" x 8" Zinc Anodes 2 Quarts Copy Cad® /Zinc Solution (Makes 3 Gals) Zinc Brightener 1 Pack Degreaser, makes 4 gallons 2 x 300W Heaters 1 x Heater Thermostat Abrasive Nylon Wheel 1 x Pump Filter/Agitator [NOT INCLUDE IN AUSTRALIAN KITS] The Caswell Plating Manual Free Technical Support 4.5 Gallon Kit: 2 x 6 Gal Plating Tank & Lid 2 x 4" x 8" Zinc Anodes 3 Quarts Copy Cad® /Zinc Solution (Makes 4.5 Gals) Zinc Brightener 2 Packs Degreaser, makes 8 gallons 2 x 300W Heaters 1 x Heater Thermostat Abrasive Nylon Wheel 1 x Pump Filter/Agitator [NOT INCLUDE IN AUSTRALIAN KITS] The Caswell Plating Manual Free Technical Support

Zinc plating is a most valuable tool when used in combating corrosion of steel.

The zinc corrodes before the steel does, sacrificing itself for the benefit of the steel. A metallurgical bond is formed between the zinc and steel forming an iron rich alloy with tenacious bond. Galvanizing can be left unpainted where it will form its own protective oxide layer.

The system requires a small DC power supply at the rate of 140 milliamps per sq inch of surface area @ 1.5 - 2 volts. The anodes supplied will plate approximately 20 square feet, or 1.85 square meters

 
Buy Now!
Price: $295.00
Choose size:
Quantity:




Contact Us:
25 Birch Court
Wyndham Vale
Victoria 3024
Phone: 03 9741 7103 or 0427 70 80 90
caswell-australia@caswellplating.com

Copyright © 2008 Caswell Australia

All Prices In Australian Dollars and Subject To Change Without Notice.

Customers Not In Australia Should Go To Caswell Inc.'s Web Site.

Customers Are Welcome To Pickup Goods From Our Location, But Please Call First To Check Product Availability
Powered by Squirrelcart © PHP Shopping Cart Software