Powder Coating System
JUST LIKE THE PROFESSIONALS!

Here is a great way to paint small parts. The process
is simple, requiring only an old electric oven to bake the finish
on.
Heres how it works!
Firstly, the surface of the part is suitably prepared, just as
you would for any other paint job.
The special gun is attached to an air compressor
(15 PSI), and a power unit. The air blows the powder from the
gun, and the power unit gives the powder a positive charge. At
the same time, the power unit is connected to the piece being
coated, and so it has a negative charge. As the positive paint
particles fly through the air, they are attracted to the part
and lay in an even layer over the entire area of the part. (This
works a little like dust on a TV screen.)
The part is then placed in an dedicated electric
oven, and baked for a while. This cures the coating to a tough
chemical resistant finish.
It is important not to use a gas oven, as the emissions
from the coating are flammable.
Why are our powder guns better than our competitors?
- Our powder cups are tapered to provide smoother flow, and
they are gravity fed, rather than siphoned.
- The charge switch is controlled by a foot pedal, leaving
your hands free - competitor's are hand controlled.
- The power pack is more compact and lighter.
- Sturdier construction - less powder leaks
Gun ships without electric plug.
- 1 Year Limited Warranty
- Input Voltage: 240volt 60HZ AC
- Fixed Output Voltage: 16KVDC
- Manual Discharge
- 2 x Powder Gun Cups
- 3 x Conical Fan Spray Pattern tips
- External High Voltage Power Supply
- In line filter
- Foot switch
- Ground Clip Cable
- Free Technical Support
|
|