| Copy
Chrome Plating Kit
Improved More Complete Kit - New, Bigger Sizes
Looks Like Chrome - Has a hint of Blue!
Hard Like Chrome - Tougher Than Nickel!
Keeps Its Shine - Just Like Chrome!
No Dangerous Chemicals - No Fumes - No Corrosive
Acids!
One coat system - eliminates
2 steps!

(Agitation Pump Not Included)
NEW! IMPROVED PERFORMANCE KIT
Larger Anodes – give more plating, with more even results
Plates up to 60 sq ft of Copy Chrome™
Simpler Instructions
New Degreaser Tank Included
New HOT heater for Degreaser included
Copy Chrome™ is a SIMPLE plating kit that provides almost
all the benefits of chromium plate - without all the hassle! The
entire plating process takes the same time as our regular nickel
plating kit, 15 minutes for indoors decorative, 30 minutes for tools,
1 hour for tough outside jobs!
The Copy Chrome™ process is ideal for all your small items
such as door handles, brackets, hinges, nuts & bolts, stamped
steel covers, etc. It can be applied to:- steel, copper, brass,
bronze, old nickel plate, and with the aid of Zincate Primer, aluminum.
All instructions and operating procedures are detailed in the Caswell
Plating Manual. Each anode will plate about 32 sq. ft of surface
area at 0.0005" before it needs to be replaced. The solution
is virtually permanent. No waste chemicals or dangerous fumes are
produced. The system operates at 0.07 amps/sq in and at 75 deg F. The customer will need to supply a small fishtank airpump to agitate the solution while plating.

1.5 Gallon Kit
- 2 x 2 Gal Plating Tank & Lids
- 2 x 6" x 8" Nickel Anodes and Bandages
- 1 x 2lb SP Degreaser (Makes 2 Gal)
- 1 Pack Copy Chrome™ Crystals with brighteners (Makes
1.5 Gal)
- 2 x 300W Heaters
- 1 x Heater Thermostat
- The Caswell Plating Manual
- Free Technical Support
|
3 Gallon Kit
- 2 x 3.5 Gal Plating Tank & Lids
- 2 x 6" x 8" Nickel Anodes and Bandages
- 2 x 2lb SP Degreaser (Makes 4 Gal)
- 2 Packs Copy Chrome™ Crystals with brighteners (Makes
3 Gal)
- 2 x 300W Heaters
- 1 x Heater Thermostat
- The Caswell Plating Manual
- Free Technical Support
|
4.5 Gallon Kit
- 2 x 6 Gal Plating Tank & Lids
- 2 x 6" x 8" Nickel Anodes and Bandages
- 2 x 2lb SP Degreaser (Makes 4 Gal)
- 3 Packs Copy Chrome™ Crystals with brighteners (Makes
4.5 Gal)
- 2 x 300W Heaters
- 1 x Heater Thermostat
- The Caswell Plating Manual
- Free Technical Support
|
Improved Brighteners
NEW!! CASWELL NICKEL/COPY CHROME™ BRIGHTENER will produce
highly ductile deposits, which are free from laminations. It produces
brilliant, white deposits of high clarity, reflectivity and depth.
The deposit is active and can be chromium plated if specified.
Superior ‘leveling’ properties enable fine scratches
and imperfections to be filled, enhancing the overall finish.
Our regular Nickel & Copy Chrome™ now plates faster
with more coverage in the low current density area. It produces
20 to 30% more thickness in the lower current density area than
any other system. If you are chrome plating onto this nickel, you
will also get better chrome coverage in the low current density
than any other nickel process.
|